enLanguage

Calcined Alumina CAS No. 1344-28-1 Used as Polishing Materials, Welding Materials and Ceramic Pigment

Calcined Alumina CAS No. 1344-28-1 Used as Polishing Materials, Welding Materials and Ceramic Pigment

Calcined Alumina CAS No. 1344-28-1 Used as Polishing Materials, Welding Materials and Ceramic Pigment

FULLN GLAZE ceramic glaze pigment Peacock Blue FU-4601 (Co-Cr blue) is a kind of blue green ceramic glaze pigment obtained by mixing, calcining and micro powder of several or more raw materials such as zinc oxide, cobalt oxide, chromium green and alumina.

Features

We have strong strength and rich experience in the Ceramic Glaze Colors Turquoise Blue, ceramic pigment suppliers, pottery pigments industry. Our company adheres to the principle of 'creating a famous brand of science and technology', focuses on the research and development of product performance, so as to better meet the needs of customers. Our product quality is reliable and is well received by the majority of users. As long as you order our products, no matter where you are, we will send professional technicians to serve you in time.

Peacock Blue FU-4601 (Co-Cr blue) 

 

CODE NO.

COLOR NAME

COLOR

COMPONENTS

Firing Temperature

CAS CODE

CERAMIC GLAZE COLORS

         

FU-4601

Peacock Blue

 

Zn-Co-Cr-Al

1050-1300℃

 68187-11-1

Product Details:

Place of Origin: China

Brand Name: FULLN

Item Code: FU-4601

Firing Temperature: 1050-1300℃

Package: 25kgs/bag, 1mt/pallet

Delivery Time: 1-2 week after order confirmed

 

Mainly usde in Tiles, Sanitary and Daily Ceramic Producing.

 

Tips:

  1. Be suitable for the colored glaze, colored drawing or pattern and under-glazedecoration. 

  2. Mixing the different pigment can get multiple colors.

  3. Fire temperature range: 1050-1300℃

  4. The component of basic glaze, the firing atmosphere, the choice of emulsion will affect the color of pigment in glaze.

 

We provide our customers with professional Calcined Alumina CAS No. 1344-28-1 Used as Polishing Materials, Welding Materials and Ceramic Pigment with sales of high-quality products as the core competitiveness and R&D as the basis for development. The business philosophy of 'prosperous in innovation, based on innovation' has penetrated into all aspects of our production and operation. The development of our enterprise has maintained a rapid and stable trend. Our company has advanced equipment and can conduct comprehensive experiments and tests on product performance.

Hot Tags: ceramic glaze pigment peacock blue, China, manufacturers, suppliers, factory, custom, wholesale, bulk, in stock, Ceramic Glaze Pigments, Ceramic Roller Printing Colors Coral Pink, black colour glass, Ceramic Glaze Pigments V Yellow, Ceramic Dry Mixed mixing Colors Cobalt Blue, Enamel Pigments Brown